Pour TheoryUnderstand the Science. Master the Craft.

Explore the library

Candle troubleshooting

Diagnose common defects by observing the symptom, testing likely causes, and recording controlled corrective changes.

Candle TunnelingCandle tunneling occurs when the flame melts only a narrow vertical shaft down the center of the candle, leaving a thick ring of unmelted solid wax adhered to the outer walls or jar perimeter.Open guideWick Mushrooming (Carbon Buildup)Mushrooming refers to a bulbous, dark carbon deposit forming at the tip of the burning wick when fuel vaporizes faster than the flame can completely oxidize it.Open guideCandle Sooting & SmokingSooting is the visible emission of unburned elemental carbon particles from the flame tip, resulting in black smoke plumes or dark soot rings inside the upper rim of candle jars.Open guideWeak Hot ThrowWeak hot throw occurs when a lit candle produces little perceptible aroma in the room despite having a noticeable cold scent or adequate fragrance oil percentage.Open guideWeak Cold ThrowWeak cold throw means an unlit candle emits little scent at room temperature when smelled up close.Open guideWet Spots (Glass Adhesion Gaps)Wet spots are not liquid moisture or fragrance oil; they are optical patches where solidified wax has pulled slightly away from the interior glass wall, leaving a micro-gap that looks like a wet blotch from outside.Open guideFrosting (Polymorphic Crystal Bloom)Frosting is a chalky, matte white crystalline layer that forms on the top, sides, or bottom of natural vegetable waxes—most noticeably soy and rapeseed waxes—as triglycerides rearrange into stable beta-polymorph crystals.Open guideSinkholes & Internal CavitiesSinkholes occur when the outer crust and surface of a candle solidify first while the hotter liquid core shrinks inward as it cools, pulling the center downward or trapping hollow cavities around the wick.Open guideWax CrackingCracking happens when uneven cooling or rigid crystalline contraction builds internal tensile stress that exceeds the wax’s structural flexibility.Open guideUneven BurningUneven burning happens when a candle consumes wax noticeably faster on one side than the other, leaving a tall unmelted ridge on the opposite wall.Open guidePoor Wick PerformancePoor wick performance encompasses erratic flame behavior—sputtering, popping, weak flicker, inconsistent curl, or inability to sustain steady combustion.Open guideExcessive Flame HeightExcessive flame height occurs when the wick supplies fuel faster than safe equilibrium, producing an elongated, unstable flame that overheats the vessel and emits smoke.Open guideWick DrowningWick drowning happens when the liquid wax melt pool rises faster than the wick can consume it—or the wick flops over—submerging the combustion zone until the flame extinguishes.Open guideSurface Imperfections (Pitting, Wrinkles & Rough Tops)Surface imperfections include dimples, bumpy cauliflower-like crusts, concentric ripples, or micro-pinholes appearing on top of freshly poured or re-solidified candles.Open guidePoor Fragrance Retention (Oil Sweating & Seepage)Poor fragrance retention ("sweating" or "syneresis") occurs when liquid fragrance oil migrates out of the solidified wax matrix and pools as oily droplets on the top surface.Open guide