Pour TheoryUnderstand the Science. Master the Craft.

Diagnostic guide

Surface Imperfections (Pitting, Wrinkles & Rough Tops)

Surface imperfections include dimples, bumpy cauliflower-like crusts, concentric ripples, or micro-pinholes appearing on top of freshly poured or re-solidified candles.

Visual appearance

Uneven, pebbled, wavy, or pitted top wax surfaces rather than a smooth level plane.

Common causes

  • Pouring too hot or too cold relative to the wax manufacturer sweet spot.
  • Cooling drafts rippling the skin as it sets.
  • Micro-bubbles trapped during vigorous fragrance mixing escaping upward as wax freezes.
  • Normal polymorphic recrystallization after burning and re-solidifying in pure 100% soy wax.

Diagnosis steps

  • Distinguish between pre-burn pouring flaws (bubbles/temperature) and post-burn rough tops (natural soy recrystallization after melting).
  • Tap the vessel gently immediately after pouring; if tiny air bubbles rise, mixing introduced excess air.

Corrective actions

  • Stir fragrance steadily with the spatula kept submerged to avoid whipping air bubbles.
  • Adjust pouring temperature in 2–3°C (5°F) increments within the wax TDS window and keep cooling rooms draft-free.
  • Use a gentle, sweeping pass of a heat gun held 15–20 cm above the surface to smooth minor pouring flaws.

What to test next

  • Run a controlled 3-temperature pour test (low, middle, high ends of TDS range) on identical vessels.

Prevention

  • Note that post-burn bumpy tops are completely normal in pure 100% soy wax; communicate this naturally or blend with coconut/paraffin if glossy re-solidification is desired.

Safety considerations

  • Keep heat guns moving continuously; localized overheating can crack thin glass rims or scorch fragrance near the surface.